在CAD/CAM系统中铣削半透明整体二氧化锆的抗断裂性能比较分析

IF 2.7 Q1 MATERIALS SCIENCE, CERAMICS
Cristian Abad-Coronel, Ángeles Paladines, A. L. Ulloa, César A. Paltán, J. I. Fajardo
{"title":"在CAD/CAM系统中铣削半透明整体二氧化锆的抗断裂性能比较分析","authors":"Cristian Abad-Coronel, Ángeles Paladines, A. L. Ulloa, César A. Paltán, J. I. Fajardo","doi":"10.3390/ceramics6020071","DOIUrl":null,"url":null,"abstract":"The aim of this study was to evaluate and compare the fracture resistance of definitive zirconia dioxide restorations obtained using a computer-aided design and manufacturing (CAD/CAM) system. Methods: Two groups of ten samples were analyzed for each material (n: 20); the first group was Zolid Gen X Amann Girrbach (ZGX) and the second group was Cercon HT Dentsply Sirona (CDS). The restorations were designed with identical parameters and milled with a CAD/CAM system. Each specimen was load tested at a speed of 0.5 mm/min, with a direction parallel to the major axis of the tooth and with an initial preload of 10 N until fracture using a universal testing machine (Universal/Tensile Testing Machine, Autograph AGS-X Series) equipped with a 20 kN load cell. The results obtained were recorded in Newtons (N), using software connected to the testing machine. Results: Statistically significant differences were found, and the fracture resistance of the monolithic zirconia crowns was lower in the CDS group (1744.84 ± 172.8 N) compared to the ZGX group (2387.41 ± 516 N). Conclusions: The monolithic zirconia CAD-CAM zirconia crowns showed sufficient fracture resistance when used in posterior molar and premolar zones with either material, as they withstood fracture loads greater than the maximum masticatory force.","PeriodicalId":33263,"journal":{"name":"Ceramics-Switzerland","volume":" ","pages":""},"PeriodicalIF":2.7000,"publicationDate":"2023-05-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Comparative Fracture Resistance Analysis of Translucent Monolithic Zirconia Dioxide Milled in a CAD/CAM System\",\"authors\":\"Cristian Abad-Coronel, Ángeles Paladines, A. L. Ulloa, César A. Paltán, J. I. Fajardo\",\"doi\":\"10.3390/ceramics6020071\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The aim of this study was to evaluate and compare the fracture resistance of definitive zirconia dioxide restorations obtained using a computer-aided design and manufacturing (CAD/CAM) system. Methods: Two groups of ten samples were analyzed for each material (n: 20); the first group was Zolid Gen X Amann Girrbach (ZGX) and the second group was Cercon HT Dentsply Sirona (CDS). The restorations were designed with identical parameters and milled with a CAD/CAM system. Each specimen was load tested at a speed of 0.5 mm/min, with a direction parallel to the major axis of the tooth and with an initial preload of 10 N until fracture using a universal testing machine (Universal/Tensile Testing Machine, Autograph AGS-X Series) equipped with a 20 kN load cell. The results obtained were recorded in Newtons (N), using software connected to the testing machine. Results: Statistically significant differences were found, and the fracture resistance of the monolithic zirconia crowns was lower in the CDS group (1744.84 ± 172.8 N) compared to the ZGX group (2387.41 ± 516 N). Conclusions: The monolithic zirconia CAD-CAM zirconia crowns showed sufficient fracture resistance when used in posterior molar and premolar zones with either material, as they withstood fracture loads greater than the maximum masticatory force.\",\"PeriodicalId\":33263,\"journal\":{\"name\":\"Ceramics-Switzerland\",\"volume\":\" \",\"pages\":\"\"},\"PeriodicalIF\":2.7000,\"publicationDate\":\"2023-05-31\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Ceramics-Switzerland\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.3390/ceramics6020071\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"MATERIALS SCIENCE, CERAMICS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Ceramics-Switzerland","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3390/ceramics6020071","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 1

摘要

本研究的目的是评估和比较使用计算机辅助设计和制造(CAD/CAM)系统获得的氧化锆修复体的抗断裂性。方法:每种材料分为两组,每组10个样品(n=20);第一组为Zolid Gen X Amann Girbach(ZGX),第二组为Cercon HT Dentsply Sirona(CDS)。修复体采用相同的参数设计,并使用CAD/CAM系统进行铣削。使用配备有20kN称重传感器的通用试验机(万能/拉伸试验机,Autograph AGS-X系列),以0.5mm/min的速度、平行于牙齿主轴的方向和10N的初始预载荷对每个试样进行载荷试验,直至断裂。使用连接到测试机的软件,将获得的结果记录在牛顿(N)中。结果:CDS组(1744.84±172.8 N)与ZGX组(2387.41±516 N)相比,整体氧化锆冠的抗断裂性较低,差异具有统计学意义。结论:整体式氧化锆CAD-CAM氧化锆冠在使用任何一种材料的后磨牙和前磨牙区域时都表现出足够的抗断裂性,因为它们能够承受大于最大咀嚼力的断裂载荷。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Comparative Fracture Resistance Analysis of Translucent Monolithic Zirconia Dioxide Milled in a CAD/CAM System
The aim of this study was to evaluate and compare the fracture resistance of definitive zirconia dioxide restorations obtained using a computer-aided design and manufacturing (CAD/CAM) system. Methods: Two groups of ten samples were analyzed for each material (n: 20); the first group was Zolid Gen X Amann Girrbach (ZGX) and the second group was Cercon HT Dentsply Sirona (CDS). The restorations were designed with identical parameters and milled with a CAD/CAM system. Each specimen was load tested at a speed of 0.5 mm/min, with a direction parallel to the major axis of the tooth and with an initial preload of 10 N until fracture using a universal testing machine (Universal/Tensile Testing Machine, Autograph AGS-X Series) equipped with a 20 kN load cell. The results obtained were recorded in Newtons (N), using software connected to the testing machine. Results: Statistically significant differences were found, and the fracture resistance of the monolithic zirconia crowns was lower in the CDS group (1744.84 ± 172.8 N) compared to the ZGX group (2387.41 ± 516 N). Conclusions: The monolithic zirconia CAD-CAM zirconia crowns showed sufficient fracture resistance when used in posterior molar and premolar zones with either material, as they withstood fracture loads greater than the maximum masticatory force.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
3.00
自引率
7.10%
发文量
66
审稿时长
10 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信