低塑性烧结激光直接能量沉积合金 IN718 的表面特性

IF 1.6 4区 材料科学 Q2 Materials Science
Mohanraj, Raja S. Thanumoorthy, Prithivirajan Sekar, A. Muthuchamy, Srikanth Bontha, A. S. S. Balan
{"title":"低塑性烧结激光直接能量沉积合金 IN718 的表面特性","authors":"Mohanraj, Raja S. Thanumoorthy, Prithivirajan Sekar, A. Muthuchamy, Srikanth Bontha, A. S. S. Balan","doi":"10.1007/s12666-024-03462-1","DOIUrl":null,"url":null,"abstract":"<p>The research work focuses on a novel post-processing sequence to improve the surface integrity and residual stress characteristics of as-printed Inconel718 (IN718) samples. The as-printed IN718 samples are subjected to solution treatment at 1050 °C, two-step precipitation hardening (@ 720 °C for 8 h and @ 620 °C for 8 h), and low plasticity burnishing. Two different sequences were attempted. Sequence-1 involves solutionizing → low plasticity burnishing followed by precipitation hardening, and sequence-2 includes solutionizing → precipitation hardening followed by low plasticity burnishing. The experimental observations and detailed investigations revealed that the samples processed via sequence 2 exhibited a better surface finish. The microhardness of the samples of sequence 2 is 10% higher than their counterparts in sequence 1. The maximum residual stress of −1375.33 MPa is obtained in sequence 1 as compared to the residual stress of −1100.67 MPa in sequence 2. The influence of the processing sequences on the surface properties has been discussed in detail using the XRD and microstructural characterization supported with EBSD analysis.</p><h3 data-test=\"abstract-sub-heading\">Graphic Abstract</h3>\n","PeriodicalId":23224,"journal":{"name":"Transactions of The Indian Institute of Metals","volume":"11 1","pages":""},"PeriodicalIF":1.6000,"publicationDate":"2024-09-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Surface Characteristics of Low Plasticity Burnished Laser Directed Energy Deposition Alloy IN718\",\"authors\":\"Mohanraj, Raja S. Thanumoorthy, Prithivirajan Sekar, A. Muthuchamy, Srikanth Bontha, A. S. S. Balan\",\"doi\":\"10.1007/s12666-024-03462-1\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The research work focuses on a novel post-processing sequence to improve the surface integrity and residual stress characteristics of as-printed Inconel718 (IN718) samples. The as-printed IN718 samples are subjected to solution treatment at 1050 °C, two-step precipitation hardening (@ 720 °C for 8 h and @ 620 °C for 8 h), and low plasticity burnishing. Two different sequences were attempted. Sequence-1 involves solutionizing → low plasticity burnishing followed by precipitation hardening, and sequence-2 includes solutionizing → precipitation hardening followed by low plasticity burnishing. The experimental observations and detailed investigations revealed that the samples processed via sequence 2 exhibited a better surface finish. The microhardness of the samples of sequence 2 is 10% higher than their counterparts in sequence 1. The maximum residual stress of −1375.33 MPa is obtained in sequence 1 as compared to the residual stress of −1100.67 MPa in sequence 2. The influence of the processing sequences on the surface properties has been discussed in detail using the XRD and microstructural characterization supported with EBSD analysis.</p><h3 data-test=\\\"abstract-sub-heading\\\">Graphic Abstract</h3>\\n\",\"PeriodicalId\":23224,\"journal\":{\"name\":\"Transactions of The Indian Institute of Metals\",\"volume\":\"11 1\",\"pages\":\"\"},\"PeriodicalIF\":1.6000,\"publicationDate\":\"2024-09-10\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Transactions of The Indian Institute of Metals\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1007/s12666-024-03462-1\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"Materials Science\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Transactions of The Indian Institute of Metals","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1007/s12666-024-03462-1","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"Materials Science","Score":null,"Total":0}
引用次数: 0

摘要

这项研究工作的重点是采用一种新颖的后处理程序来改善轧制 Inconel718 (IN718) 样品的表面完整性和残余应力特性。印模 IN718 样品在 1050 °C 下进行固溶处理、两步沉淀硬化(720 °C 8 小时和 620 °C 8 小时)和低塑性抛光。尝试了两种不同的顺序。顺序-1 包括固溶 → 低塑性抛光,然后沉淀硬化;顺序-2 包括固溶 → 沉淀硬化,然后低塑性抛光。实验观察和详细调查显示,通过序列 2 加工的样品具有更好的表面光洁度。序列 2 样品的显微硬度比序列 1 高 10%。序列 1 得到的最大残余应力为 -1375.33 兆帕,而序列 2 得到的残余应力为 -1100.67 兆帕。在 EBSD 分析的支持下,利用 XRD 和微结构表征详细讨论了加工顺序对表面特性的影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Surface Characteristics of Low Plasticity Burnished Laser Directed Energy Deposition Alloy IN718

Surface Characteristics of Low Plasticity Burnished Laser Directed Energy Deposition Alloy IN718

The research work focuses on a novel post-processing sequence to improve the surface integrity and residual stress characteristics of as-printed Inconel718 (IN718) samples. The as-printed IN718 samples are subjected to solution treatment at 1050 °C, two-step precipitation hardening (@ 720 °C for 8 h and @ 620 °C for 8 h), and low plasticity burnishing. Two different sequences were attempted. Sequence-1 involves solutionizing → low plasticity burnishing followed by precipitation hardening, and sequence-2 includes solutionizing → precipitation hardening followed by low plasticity burnishing. The experimental observations and detailed investigations revealed that the samples processed via sequence 2 exhibited a better surface finish. The microhardness of the samples of sequence 2 is 10% higher than their counterparts in sequence 1. The maximum residual stress of −1375.33 MPa is obtained in sequence 1 as compared to the residual stress of −1100.67 MPa in sequence 2. The influence of the processing sequences on the surface properties has been discussed in detail using the XRD and microstructural characterization supported with EBSD analysis.

Graphic Abstract

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Transactions of The Indian Institute of Metals
Transactions of The Indian Institute of Metals Materials Science-Metals and Alloys
CiteScore
2.60
自引率
6.20%
发文量
3
期刊介绍: Transactions of the Indian Institute of Metals publishes original research articles and reviews on ferrous and non-ferrous process metallurgy, structural and functional materials development, physical, chemical and mechanical metallurgy, welding science and technology, metal forming, particulate technologies, surface engineering, characterization of materials, thermodynamics and kinetics, materials modelling and other allied branches of Metallurgy and Materials Engineering. Transactions of the Indian Institute of Metals also serves as a forum for rapid publication of recent advances in all the branches of Metallurgy and Materials Engineering. The technical content of the journal is scrutinized by the Editorial Board composed of experts from various disciplines of Metallurgy and Materials Engineering. Editorial Advisory Board provides valuable advice on technical matters related to the publication of Transactions.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信