{"title":"铝箔夹层对 6061 铝合金真空扩散粘接接头性能的影响","authors":"Da-shuang Liu, Jian-hua Xu, Xiong-hui Li, Ping Wei, Yun Liang, Jian Qin, Hua-wei Sun, Tian-ran Ding, Zong-ye Ding, Su-juan Zhong, Lei Zhang, Wei-min Long","doi":"10.1007/s42243-024-01302-6","DOIUrl":null,"url":null,"abstract":"<p>The vacuum diffusion bonding method was used to introduce Al foil as the middle layer, and 6061 aluminium alloy was vacuum diffusion bonding together. The typical microstructure characteristics and mechanical properties of 6061/Al/6061 welded joints were studied in detail, the effects of process parameters and Al intermediate layer on the microstructure and mechanical properties were revealed, and the diffusion bonding mechanism of 6061/Al/6061 welded joints was described. Al foil middle layer welded joint had the best performance at the temperature of 540 °C, the holding time of 120 min, and the welding pressure of 4 MPa. The bonding ratio is 95.91%, the shear strength is 79 MPa, and the deformation rate is 8.05%, and the introduction of Al intermediate layer improves the element distribution and microstructure, so that the bonding ratio of the welded joint is increased by 10.86%, the shear strength is increased by 5.55 MPa, and the deformation rate is reduced by 1.58%. The fracture morphology has typical ductile fracture characteristics.</p>","PeriodicalId":16151,"journal":{"name":"Journal of Iron and Steel Research International","volume":null,"pages":null},"PeriodicalIF":2.5000,"publicationDate":"2024-08-12","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Influence of Al foil interlayer on performance of vacuum diffusion bonding joint of 6061 aluminium alloy\",\"authors\":\"Da-shuang Liu, Jian-hua Xu, Xiong-hui Li, Ping Wei, Yun Liang, Jian Qin, Hua-wei Sun, Tian-ran Ding, Zong-ye Ding, Su-juan Zhong, Lei Zhang, Wei-min Long\",\"doi\":\"10.1007/s42243-024-01302-6\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The vacuum diffusion bonding method was used to introduce Al foil as the middle layer, and 6061 aluminium alloy was vacuum diffusion bonding together. The typical microstructure characteristics and mechanical properties of 6061/Al/6061 welded joints were studied in detail, the effects of process parameters and Al intermediate layer on the microstructure and mechanical properties were revealed, and the diffusion bonding mechanism of 6061/Al/6061 welded joints was described. Al foil middle layer welded joint had the best performance at the temperature of 540 °C, the holding time of 120 min, and the welding pressure of 4 MPa. The bonding ratio is 95.91%, the shear strength is 79 MPa, and the deformation rate is 8.05%, and the introduction of Al intermediate layer improves the element distribution and microstructure, so that the bonding ratio of the welded joint is increased by 10.86%, the shear strength is increased by 5.55 MPa, and the deformation rate is reduced by 1.58%. The fracture morphology has typical ductile fracture characteristics.</p>\",\"PeriodicalId\":16151,\"journal\":{\"name\":\"Journal of Iron and Steel Research International\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":2.5000,\"publicationDate\":\"2024-08-12\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Iron and Steel Research International\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1007/s42243-024-01302-6\",\"RegionNum\":2,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Iron and Steel Research International","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1007/s42243-024-01302-6","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

采用真空扩散粘接法引入铝箔作为中间层,与 6061 铝合金进行真空扩散粘接。详细研究了 6061/Al/6061 焊接接头的典型显微组织特征和力学性能,揭示了工艺参数和铝中间层对显微组织和力学性能的影响,并阐述了 6061/Al/6061 焊接接头的扩散结合机理。在温度为 540 ℃、保温时间为 120 min、焊接压力为 4 MPa 的条件下,铝箔中间层焊接接头的性能最佳。铝中间层的引入改善了元素分布和微观结构,使焊接接头的结合率提高了 10.86%,剪切强度提高了 5.55 MPa,变形率降低了 1.58%。断口形态具有典型的韧性断口特征。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Influence of Al foil interlayer on performance of vacuum diffusion bonding joint of 6061 aluminium alloy

Influence of Al foil interlayer on performance of vacuum diffusion bonding joint of 6061 aluminium alloy

The vacuum diffusion bonding method was used to introduce Al foil as the middle layer, and 6061 aluminium alloy was vacuum diffusion bonding together. The typical microstructure characteristics and mechanical properties of 6061/Al/6061 welded joints were studied in detail, the effects of process parameters and Al intermediate layer on the microstructure and mechanical properties were revealed, and the diffusion bonding mechanism of 6061/Al/6061 welded joints was described. Al foil middle layer welded joint had the best performance at the temperature of 540 °C, the holding time of 120 min, and the welding pressure of 4 MPa. The bonding ratio is 95.91%, the shear strength is 79 MPa, and the deformation rate is 8.05%, and the introduction of Al intermediate layer improves the element distribution and microstructure, so that the bonding ratio of the welded joint is increased by 10.86%, the shear strength is increased by 5.55 MPa, and the deformation rate is reduced by 1.58%. The fracture morphology has typical ductile fracture characteristics.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
16.00%
发文量
161
审稿时长
2.8 months
期刊介绍: Publishes critically reviewed original research of archival significance Covers hydrometallurgy, pyrometallurgy, electrometallurgy, transport phenomena, process control, physical chemistry, solidification, mechanical working, solid state reactions, materials processing, and more Includes welding & joining, surface treatment, mathematical modeling, corrosion, wear and abrasion Journal of Iron and Steel Research International publishes original papers and occasional invited reviews on aspects of research and technology in the process metallurgy and metallic materials. Coverage emphasizes the relationships among the processing, structure and properties of metals, including advanced steel materials, superalloy, intermetallics, metallic functional materials, powder metallurgy, structural titanium alloy, composite steel materials, high entropy alloy, amorphous alloys, metallic nanomaterials, etc..
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信