利用水冶法从废铜中合成碳酸铜

Tika Paramitha
{"title":"利用水冶法从废铜中合成碳酸铜","authors":"Tika Paramitha","doi":"10.20961/esta.v3i1.78985","DOIUrl":null,"url":null,"abstract":"Electronic waste in Indonesia continues to increase, electronic waste is categorized as B3 waste which can threaten the environment. Electronic waste contains metals that can berecovery namely 20% copper (Cu), 8% iron (Fe), 4% tin (Sn), 2% nickel (Ni), 2% lead (Pb), 1% zinc (Zn), 0.2% silver (Ag), 0.1% gold (Au) and 0.005% palladium (Pa). Copper can be used as a raw material for making pigments mountain blue. Pigment extraction from copper metal can be done using the hydrometallurgical method which is considered more environmentally friendly and economical. The hydrometallurgical method uses solvents in the liquid phase to dissolve copper metal from waste and convert it into the desired compound. The materials used to make mountain blue pigment are copper waste, sulfuric acid (H2SO4), sodium hydroxide (NaOH), sodium carbonate (Na2CO3), hydrogen peroxide (H2O2), and distilled water. Meanwhile, the materials used for pigment application are Carboxymethyl Cellulose (CMC) and titanium dioxide (TiO2). In this process, washing or leaching will be carried out(leaching) namely a chemical concentration process to release ore impurities from a mineral by dissolving it using certain reagents. Factors that influence the metal leaching process are temperature and acid concentration. In this experiment, the hydrometallurgical method succeeded in processing electronic waste into a blue pigment (mountain blue). The average pigment yield mountain blue in this experiment it was 1.25 grams of montain blue/gram of copper. Furthermore, the average conversion of pigment  mountain blue was 89.3%.","PeriodicalId":11676,"journal":{"name":"Energy Storage Technology and Applications","volume":"40 7","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-02-06","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Synthesis of Copper Carbonate from Copper Waste Using the Hydrometallurgical Method\",\"authors\":\"Tika Paramitha\",\"doi\":\"10.20961/esta.v3i1.78985\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Electronic waste in Indonesia continues to increase, electronic waste is categorized as B3 waste which can threaten the environment. Electronic waste contains metals that can berecovery namely 20% copper (Cu), 8% iron (Fe), 4% tin (Sn), 2% nickel (Ni), 2% lead (Pb), 1% zinc (Zn), 0.2% silver (Ag), 0.1% gold (Au) and 0.005% palladium (Pa). Copper can be used as a raw material for making pigments mountain blue. Pigment extraction from copper metal can be done using the hydrometallurgical method which is considered more environmentally friendly and economical. The hydrometallurgical method uses solvents in the liquid phase to dissolve copper metal from waste and convert it into the desired compound. The materials used to make mountain blue pigment are copper waste, sulfuric acid (H2SO4), sodium hydroxide (NaOH), sodium carbonate (Na2CO3), hydrogen peroxide (H2O2), and distilled water. Meanwhile, the materials used for pigment application are Carboxymethyl Cellulose (CMC) and titanium dioxide (TiO2). In this process, washing or leaching will be carried out(leaching) namely a chemical concentration process to release ore impurities from a mineral by dissolving it using certain reagents. Factors that influence the metal leaching process are temperature and acid concentration. In this experiment, the hydrometallurgical method succeeded in processing electronic waste into a blue pigment (mountain blue). The average pigment yield mountain blue in this experiment it was 1.25 grams of montain blue/gram of copper. Furthermore, the average conversion of pigment  mountain blue was 89.3%.\",\"PeriodicalId\":11676,\"journal\":{\"name\":\"Energy Storage Technology and Applications\",\"volume\":\"40 7\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2024-02-06\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Energy Storage Technology and Applications\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.20961/esta.v3i1.78985\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Energy Storage Technology and Applications","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.20961/esta.v3i1.78985","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

印度尼西亚的电子垃圾持续增加,电子垃圾被归类为 B3 类垃圾,会对环境造成威胁。电子垃圾中含有可回收的金属,即 20% 的铜(Cu)、8% 的铁(Fe)、4% 的锡(Sn)、2% 的镍(Ni)、2% 的铅(Pb)、1% 的锌(Zn)、0.2% 的银(Ag)、0.1% 的金(Au)和 0.005% 的钯(Pa)。铜可用作制作山蓝颜料的原料。从金属铜中提取颜料可采用水冶法,这种方法被认为更环保、更经济。湿法冶金法在液相中使用溶剂溶解废料中的金属铜,并将其转化为所需的化合物。制作山蓝颜料的材料包括铜废料、硫酸(H2SO4)、氢氧化钠(NaOH)、碳酸钠(Na2CO3)、过氧化氢(H2O2)和蒸馏水。同时,用于颜料应用的材料是羧甲基纤维素(CMC)和二氧化钛(TiO2)。在这一过程中,将进行洗涤或浸出(浸出),即通过使用某些试剂溶解矿石来释放矿石杂质的化学浓缩过程。影响金属浸出过程的因素是温度和酸浓度。在本实验中,水冶法成功地将电子废料加工成了蓝色颜料(山蓝)。本实验中山蓝的平均颜料产量为 1.25 克山蓝/克铜。此外,颜料山蓝的平均转化率为 89.3%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Synthesis of Copper Carbonate from Copper Waste Using the Hydrometallurgical Method
Electronic waste in Indonesia continues to increase, electronic waste is categorized as B3 waste which can threaten the environment. Electronic waste contains metals that can berecovery namely 20% copper (Cu), 8% iron (Fe), 4% tin (Sn), 2% nickel (Ni), 2% lead (Pb), 1% zinc (Zn), 0.2% silver (Ag), 0.1% gold (Au) and 0.005% palladium (Pa). Copper can be used as a raw material for making pigments mountain blue. Pigment extraction from copper metal can be done using the hydrometallurgical method which is considered more environmentally friendly and economical. The hydrometallurgical method uses solvents in the liquid phase to dissolve copper metal from waste and convert it into the desired compound. The materials used to make mountain blue pigment are copper waste, sulfuric acid (H2SO4), sodium hydroxide (NaOH), sodium carbonate (Na2CO3), hydrogen peroxide (H2O2), and distilled water. Meanwhile, the materials used for pigment application are Carboxymethyl Cellulose (CMC) and titanium dioxide (TiO2). In this process, washing or leaching will be carried out(leaching) namely a chemical concentration process to release ore impurities from a mineral by dissolving it using certain reagents. Factors that influence the metal leaching process are temperature and acid concentration. In this experiment, the hydrometallurgical method succeeded in processing electronic waste into a blue pigment (mountain blue). The average pigment yield mountain blue in this experiment it was 1.25 grams of montain blue/gram of copper. Furthermore, the average conversion of pigment  mountain blue was 89.3%.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信