Iori Kojima, C. Iwamoto, Yuka Shimizu, T. Matsuda, A. Hirose
{"title":"通过 FSSW 多步加载工艺连接的铝合金和镀锌钢板界面的微观结构","authors":"Iori Kojima, C. Iwamoto, Yuka Shimizu, T. Matsuda, A. Hirose","doi":"10.1080/09507116.2023.2230650","DOIUrl":null,"url":null,"abstract":"Abstract When joining between GA980 and A6061 plates by the FSSW, brittle intermetallic compounds and Zn-contained region are formed at the joint interface. These local reaction products determine the strength of the joint. Therefore, the bonding interface microstructure analysis is crucial to control the process and improve strength. This study performed microstructural analysis near the joint interface on GA980/A6061 joints bonded by the FSSW. The detailed variation of the IMC thickness along with the bonded interface and the microstructure of the Zn-contained region in A6061 plate was clarified. In the A6061 plate, a simple shear texture was observed with the Al <110> direction in the tool rotational direction and the Al {111} plane perpendicular to the direction of the elongated grains. In elongated Al grains surrounded by high-angle grain boundaries, the grains were divided by the low-angle grain boundaries.","PeriodicalId":23605,"journal":{"name":"Welding International","volume":"2018 1","pages":"655 - 665"},"PeriodicalIF":0.0000,"publicationDate":"2023-07-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Microstructure of the interface between aluminum alloy and galvannealed steel plates jointed by FSSW multi-step loading process\",\"authors\":\"Iori Kojima, C. Iwamoto, Yuka Shimizu, T. Matsuda, A. Hirose\",\"doi\":\"10.1080/09507116.2023.2230650\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Abstract When joining between GA980 and A6061 plates by the FSSW, brittle intermetallic compounds and Zn-contained region are formed at the joint interface. These local reaction products determine the strength of the joint. Therefore, the bonding interface microstructure analysis is crucial to control the process and improve strength. This study performed microstructural analysis near the joint interface on GA980/A6061 joints bonded by the FSSW. The detailed variation of the IMC thickness along with the bonded interface and the microstructure of the Zn-contained region in A6061 plate was clarified. In the A6061 plate, a simple shear texture was observed with the Al <110> direction in the tool rotational direction and the Al {111} plane perpendicular to the direction of the elongated grains. In elongated Al grains surrounded by high-angle grain boundaries, the grains were divided by the low-angle grain boundaries.\",\"PeriodicalId\":23605,\"journal\":{\"name\":\"Welding International\",\"volume\":\"2018 1\",\"pages\":\"655 - 665\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-07-21\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Welding International\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1080/09507116.2023.2230650\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"Materials Science\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Welding International","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/09507116.2023.2230650","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Materials Science","Score":null,"Total":0}
Microstructure of the interface between aluminum alloy and galvannealed steel plates jointed by FSSW multi-step loading process
Abstract When joining between GA980 and A6061 plates by the FSSW, brittle intermetallic compounds and Zn-contained region are formed at the joint interface. These local reaction products determine the strength of the joint. Therefore, the bonding interface microstructure analysis is crucial to control the process and improve strength. This study performed microstructural analysis near the joint interface on GA980/A6061 joints bonded by the FSSW. The detailed variation of the IMC thickness along with the bonded interface and the microstructure of the Zn-contained region in A6061 plate was clarified. In the A6061 plate, a simple shear texture was observed with the Al <110> direction in the tool rotational direction and the Al {111} plane perpendicular to the direction of the elongated grains. In elongated Al grains surrounded by high-angle grain boundaries, the grains were divided by the low-angle grain boundaries.
期刊介绍:
Welding International provides comprehensive English translations of complete articles, selected from major international welding journals, including: Journal of Japan Welding Society - Japan Journal of Light Metal Welding and Construction - Japan Przeglad Spawalnictwa - Poland Quarterly Journal of Japan Welding Society - Japan Revista de Metalurgia - Spain Rivista Italiana della Saldatura - Italy Soldagem & Inspeção - Brazil Svarochnoe Proizvodstvo - Russia Welding International is a well-established and widely respected journal and the translators are carefully chosen with each issue containing a balanced selection of between 15 and 20 articles. The articles cover research techniques, equipment and process developments, applications and material and are not available elsewhere in English. This journal provides a valuable and unique service for those needing to keep up-to-date on the latest developments in welding technology in non-English speaking countries.