{"title":"[用扫描电子显微镜(SEM)研究汞合金和玻璃陶瓷水泥的不同抛光工艺]。","authors":"A Kakaboura,&nbsp;G Vougiouklakis,&nbsp;G Argiri","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>Finishing and polishing an amalgam restoration, is considered as an important and necessary step of the restorative procedure. Various polishing techniques have been recommended to success a smooth amalgam surface. The aim of this study was to investigate the influence of three different polishing treatments on the marginal integrity and surface smoothness of restorations made of three commercially available amalgams and a glass-cermet cement. The materials used were the amalgams, Amalcap (Vivadent), Dispersalloy (Johnson and Johnson), Duralloy (Degussa) and the glass-cermet Katac-Silver (ESPE). The occlusal surfaces of the restorations were polished by the methods: I) round bur, No4-rubber cup-zinc oxide paste in a small brush, II) round bur No 4-bur-brown, green and super green (Shofu) polishing cups and points successively and III) amalgam polishing bur of 12-blades-smooth amalgam polishing bur. Photographs from unpolished and polished surfaces of the restorations, were taken with scanning electron microscope, to evaluate the polishing techniques. An improvement of marginal integrity and surface smoothness of all amalgam restorations was observed after the specimens had been polished with the three techniques. Method II, included Shofu polishers, proved the best results in comparison to the methods I and III. Polishing of glass-cermet cement was impossible with the examined techniques.</p>","PeriodicalId":75901,"journal":{"name":"Hellenika stomatologika chronika. Hellenic stomatological annals","volume":"33 4","pages":"217-25"},"PeriodicalIF":0.0000,"publicationDate":"1989-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"[A study of different polishing techniques for amalgams and glass-cermet cement by scanning electron microscope (SEM)].\",\"authors\":\"A Kakaboura,&nbsp;G Vougiouklakis,&nbsp;G Argiri\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>Finishing and polishing an amalgam restoration, is considered as an important and necessary step of the restorative procedure. Various polishing techniques have been recommended to success a smooth amalgam surface. The aim of this study was to investigate the influence of three different polishing treatments on the marginal integrity and surface smoothness of restorations made of three commercially available amalgams and a glass-cermet cement. The materials used were the amalgams, Amalcap (Vivadent), Dispersalloy (Johnson and Johnson), Duralloy (Degussa) and the glass-cermet Katac-Silver (ESPE). The occlusal surfaces of the restorations were polished by the methods: I) round bur, No4-rubber cup-zinc oxide paste in a small brush, II) round bur No 4-bur-brown, green and super green (Shofu) polishing cups and points successively and III) amalgam polishing bur of 12-blades-smooth amalgam polishing bur. Photographs from unpolished and polished surfaces of the restorations, were taken with scanning electron microscope, to evaluate the polishing techniques. An improvement of marginal integrity and surface smoothness of all amalgam restorations was observed after the specimens had been polished with the three techniques. Method II, included Shofu polishers, proved the best results in comparison to the methods I and III. Polishing of glass-cermet cement was impossible with the examined techniques.</p>\",\"PeriodicalId\":75901,\"journal\":{\"name\":\"Hellenika stomatologika chronika. Hellenic stomatological annals\",\"volume\":\"33 4\",\"pages\":\"217-25\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1989-10-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Hellenika stomatologika chronika. Hellenic stomatological annals\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Hellenika stomatologika chronika. Hellenic stomatological annals","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

银汞合金修复体的整理和抛光是修复过程中重要而必要的步骤。各种抛光技术已被推荐成功一个光滑的银汞合金表面。本研究的目的是研究三种不同的抛光处理对三种市售汞合金和玻璃陶瓷水泥制成的修复体的边缘完整性和表面光滑度的影响。使用的材料是汞合金,Amalcap (Vivadent), Dispersalloy (Johnson and Johnson), Duralloy (Degussa)和玻璃陶瓷Katac-Silver (ESPE)。修复体咬合表面的抛光方法为:1)圆钎、4号橡胶杯-小刷氧化锌膏;2)4号圆钎-棕色、绿色和超绿色(Shofu)抛光杯和抛光点;3)12刃银汞合金抛光钎-光滑银汞合金抛光钎。用扫描电子显微镜对修复体的未抛光和抛光表面进行了拍摄,以评估抛光技术。所有汞合金修复体的边缘完整性和表面光滑度在用三种技术抛光后都得到了改善。方法二,包括Shofu抛光剂,与方法一和方法三相比,证明了最好的结果。对玻璃陶瓷水泥进行抛光是不可能的。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
[A study of different polishing techniques for amalgams and glass-cermet cement by scanning electron microscope (SEM)].

Finishing and polishing an amalgam restoration, is considered as an important and necessary step of the restorative procedure. Various polishing techniques have been recommended to success a smooth amalgam surface. The aim of this study was to investigate the influence of three different polishing treatments on the marginal integrity and surface smoothness of restorations made of three commercially available amalgams and a glass-cermet cement. The materials used were the amalgams, Amalcap (Vivadent), Dispersalloy (Johnson and Johnson), Duralloy (Degussa) and the glass-cermet Katac-Silver (ESPE). The occlusal surfaces of the restorations were polished by the methods: I) round bur, No4-rubber cup-zinc oxide paste in a small brush, II) round bur No 4-bur-brown, green and super green (Shofu) polishing cups and points successively and III) amalgam polishing bur of 12-blades-smooth amalgam polishing bur. Photographs from unpolished and polished surfaces of the restorations, were taken with scanning electron microscope, to evaluate the polishing techniques. An improvement of marginal integrity and surface smoothness of all amalgam restorations was observed after the specimens had been polished with the three techniques. Method II, included Shofu polishers, proved the best results in comparison to the methods I and III. Polishing of glass-cermet cement was impossible with the examined techniques.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信