{"title":"[牙套黏合剂与钛铸件的结合强度]。","authors":"Y Hibino,&nbsp;A Kuroiwa,&nbsp;S Kurosawa,&nbsp;S Kanke,&nbsp;H Hashimoto","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>This study compared the tensile bond strength of dental luting cements to the titanium castings with gold alloy (Type IV), 12% Au-Ag-Pd alloy and Ni-Cr alloy in dental clinical practice. In this experimental condition, the zinc phosphate cement did not adhere to any dental casting alloy tested. The tensile bond strength of polycarboxylate cement to the titanium castings was 96 kg/cm2, about two times as high as that gold alloy (Type IV). The tensile bond strength of the glass ionomer cement to titanium castings was 32 kg/cm2, about two times as high as that of dental precious alloys. The tensile bond strength of the adhesive resin cement to titanium castings was 220 kg/cm2, about three times as high as that of dental precious alloys.</p>","PeriodicalId":77622,"journal":{"name":"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"1990-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"[Bond strength of dental luting cements to titanium castings].\",\"authors\":\"Y Hibino,&nbsp;A Kuroiwa,&nbsp;S Kurosawa,&nbsp;S Kanke,&nbsp;H Hashimoto\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>This study compared the tensile bond strength of dental luting cements to the titanium castings with gold alloy (Type IV), 12% Au-Ag-Pd alloy and Ni-Cr alloy in dental clinical practice. In this experimental condition, the zinc phosphate cement did not adhere to any dental casting alloy tested. The tensile bond strength of polycarboxylate cement to the titanium castings was 96 kg/cm2, about two times as high as that gold alloy (Type IV). The tensile bond strength of the glass ionomer cement to titanium castings was 32 kg/cm2, about two times as high as that of dental precious alloys. The tensile bond strength of the adhesive resin cement to titanium castings was 220 kg/cm2, about three times as high as that of dental precious alloys.</p>\",\"PeriodicalId\":77622,\"journal\":{\"name\":\"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1990-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

本研究比较了牙科临床应用中牙套水泥与含金合金(IV型)、12% Au-Ag-Pd合金和Ni-Cr合金的钛铸件的抗拉强度。在本实验条件下,磷酸锌水泥不粘附任何牙科铸造合金。聚羧酸盐水门汀对钛铸件的抗拉结合强度为96 kg/cm2,约为IV型金合金的2倍;玻璃离子水门汀对钛铸件的抗拉结合强度为32 kg/cm2,约为牙用贵重合金的2倍。胶粘剂树脂水泥与钛铸件的抗拉强度为220 kg/cm2,约为牙用贵重合金的3倍。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
[Bond strength of dental luting cements to titanium castings].

This study compared the tensile bond strength of dental luting cements to the titanium castings with gold alloy (Type IV), 12% Au-Ag-Pd alloy and Ni-Cr alloy in dental clinical practice. In this experimental condition, the zinc phosphate cement did not adhere to any dental casting alloy tested. The tensile bond strength of polycarboxylate cement to the titanium castings was 96 kg/cm2, about two times as high as that gold alloy (Type IV). The tensile bond strength of the glass ionomer cement to titanium castings was 32 kg/cm2, about two times as high as that of dental precious alloys. The tensile bond strength of the adhesive resin cement to titanium castings was 220 kg/cm2, about three times as high as that of dental precious alloys.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信