{"title":"复合材料管对接接头激光焊接技术的发展","authors":"Radosław Ciokan, Michał Urbańczyk","doi":"10.17729/EBIS.2021.1/2","DOIUrl":null,"url":null,"abstract":"The article presents the results concerning the development of a technology combining laser welding and hybrid surfacing enabling the making of butt joints in composite tube grades Sanicro 38/4L7 and 3R12/4L7. The tests involved the determination of the parameters of the laser welding of tube grade 4L7 and the hybrid surfacing of the external layer of tube grade Sanicro 38 and 3R12. The article also presents the results of the macro and microscopic tests of the joints.","PeriodicalId":184101,"journal":{"name":"Biuletyn Instytutu Spawalnictwa","volume":"4 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2021-02-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"The Development of a Technology of the Laser-Based Welding of Butt Joints in Composite Tubes\",\"authors\":\"Radosław Ciokan, Michał Urbańczyk\",\"doi\":\"10.17729/EBIS.2021.1/2\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The article presents the results concerning the development of a technology combining laser welding and hybrid surfacing enabling the making of butt joints in composite tube grades Sanicro 38/4L7 and 3R12/4L7. The tests involved the determination of the parameters of the laser welding of tube grade 4L7 and the hybrid surfacing of the external layer of tube grade Sanicro 38 and 3R12. The article also presents the results of the macro and microscopic tests of the joints.\",\"PeriodicalId\":184101,\"journal\":{\"name\":\"Biuletyn Instytutu Spawalnictwa\",\"volume\":\"4 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-02-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Biuletyn Instytutu Spawalnictwa\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.17729/EBIS.2021.1/2\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Biuletyn Instytutu Spawalnictwa","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17729/EBIS.2021.1/2","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
The Development of a Technology of the Laser-Based Welding of Butt Joints in Composite Tubes
The article presents the results concerning the development of a technology combining laser welding and hybrid surfacing enabling the making of butt joints in composite tube grades Sanicro 38/4L7 and 3R12/4L7. The tests involved the determination of the parameters of the laser welding of tube grade 4L7 and the hybrid surfacing of the external layer of tube grade Sanicro 38 and 3R12. The article also presents the results of the macro and microscopic tests of the joints.