{"title":"The Dependence of Secondary Dendrite Arm Spacing on Solidification Conditions—II. Al-7 Si-0.5 Mg Alloys treated with Sr and Sb","authors":"Q. S. Hamed, R. Elliott","doi":"10.1080/09534962.1993.11819125","DOIUrl":null,"url":null,"abstract":"AbstractSteady-state directional solidification studies are described for Sr- and Sb-treated commercial purity Al-7 Si-0.5 Mg (LM25) casting alloys. The minor additions refine the secondary dendrit...","PeriodicalId":9691,"journal":{"name":"Cast Metals","volume":"90 1","pages":"42-46"},"PeriodicalIF":0.0000,"publicationDate":"1993-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"6","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Cast Metals","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/09534962.1993.11819125","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 6
Abstract
AbstractSteady-state directional solidification studies are described for Sr- and Sb-treated commercial purity Al-7 Si-0.5 Mg (LM25) casting alloys. The minor additions refine the secondary dendrit...