Ionic Conductivity and Power Conversion Efficiency Study of KI Incorporated Glucosyl Carboxonium Ion-based Biopolymer Crust Electrolyte

Q2 Materials Science
E. Bementa, G. Okram, M. Rajan
{"title":"Ionic Conductivity and Power Conversion Efficiency Study of KI Incorporated Glucosyl Carboxonium Ion-based Biopolymer Crust Electrolyte","authors":"E. Bementa, G. Okram, M. Rajan","doi":"10.1080/03602559.2017.1381245","DOIUrl":null,"url":null,"abstract":"The impedance of well-characterized KI-incorporated glucosyl carboxonium ion-based biopolymer crust electrolytes up to a maximum 2.7 wt% was measured using electrical impedance spectroscopy. Enhanced ionic conductivity of 2.3657 × 10−2 S cm−1 on the addition of 2.7 wt% of KI was observed in contrast to earlier reported value for pure GCI of 4.5278 × 10−4 S cm−1. This is attributed due to the increased concentration of KI in the system and is corroborated with increased ion density (n), mobility (µ), and diffusion coefficients (D). Dielectric and modulus study shows the capacitive nature of electrolyte. Fabricated dye-sensitized solar cell using pure glucosyl carboxonium ion crust and KI-incorporated glucosyl carboxonium ion crust shows the efficiency of 1.19% for pure and shows the efficiency of 2.14% for 2.6 wt% of KI in glucosyl carboxonium ion at 1 sun condition.","PeriodicalId":20629,"journal":{"name":"Polymer-Plastics Technology and Engineering","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2018-09-02","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Polymer-Plastics Technology and Engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/03602559.2017.1381245","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"Materials Science","Score":null,"Total":0}
引用次数: 2

Abstract

The impedance of well-characterized KI-incorporated glucosyl carboxonium ion-based biopolymer crust electrolytes up to a maximum 2.7 wt% was measured using electrical impedance spectroscopy. Enhanced ionic conductivity of 2.3657 × 10−2 S cm−1 on the addition of 2.7 wt% of KI was observed in contrast to earlier reported value for pure GCI of 4.5278 × 10−4 S cm−1. This is attributed due to the increased concentration of KI in the system and is corroborated with increased ion density (n), mobility (µ), and diffusion coefficients (D). Dielectric and modulus study shows the capacitive nature of electrolyte. Fabricated dye-sensitized solar cell using pure glucosyl carboxonium ion crust and KI-incorporated glucosyl carboxonium ion crust shows the efficiency of 1.19% for pure and shows the efficiency of 2.14% for 2.6 wt% of KI in glucosyl carboxonium ion at 1 sun condition.
KI掺入葡萄糖基羧基离子基生物聚合物结壳电解质的离子电导率和功率转换效率研究
利用电阻抗谱法测量了表征良好的ki -葡萄糖基羧基离子基生物聚合物外壳电解质的阻抗,最大可达2.7 wt%。与之前报道的纯GCI的4.5278 × 10−4 S cm−1相比,在添加2.7 wt%的KI时,离子电导率提高了2.3657 × 10−2 S cm−1。这是由于系统中KI浓度的增加,离子密度(n)、迁移率(µ)和扩散系数(D)的增加也证实了这一点。介电和模量研究显示了电解质的电容性。在1个太阳条件下,用纯葡萄糖基碳鎓离子壳和KI掺杂的葡萄糖基碳鎓离子壳制备的染料敏化太阳能电池,纯葡萄糖基碳鎓离子壳的效率为1.19%,KI掺杂2.6 wt%葡萄糖基碳鎓离子壳的效率为2.14%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Polymer-Plastics Technology and Engineering
Polymer-Plastics Technology and Engineering 工程技术-高分子科学
CiteScore
1.71
自引率
0.00%
发文量
0
审稿时长
4 months
文献相关原料
公司名称 产品信息 采购帮参考价格
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信