{"title":"A new study on the superplasticity of TiAl alloys","authors":"Run Xu, Boyong Hur","doi":"10.30564/opmr.v2i1.1869","DOIUrl":null,"url":null,"abstract":"The superplasticity of Ti-46.7Al-2.2Cr(at.%) alloy was studied by mathematical induction. It is found that Zener Hollomon relative formula and there are serious deflections. According to the true superplastic stress and true strain curves, the deflection values of n=-7.46 and B=1439MPa are obtained, indicating that the limit of n>0 has been exceeded, which needs to be characterized by a negative sign. This shows that it conforms to the principle that the smaller n is, the better superplasticity is, but the problem that it has become a negative number needs to attract the attention of peers meantime B is a better match. ","PeriodicalId":19583,"journal":{"name":"Organic Polymer Material Research","volume":"30 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2020-05-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Organic Polymer Material Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30564/opmr.v2i1.1869","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The superplasticity of Ti-46.7Al-2.2Cr(at.%) alloy was studied by mathematical induction. It is found that Zener Hollomon relative formula and there are serious deflections. According to the true superplastic stress and true strain curves, the deflection values of n=-7.46 and B=1439MPa are obtained, indicating that the limit of n>0 has been exceeded, which needs to be characterized by a negative sign. This shows that it conforms to the principle that the smaller n is, the better superplasticity is, but the problem that it has become a negative number needs to attract the attention of peers meantime B is a better match. 
TiAl合金超塑性的新研究
采用数学归纳法研究了Ti-46.7Al-2.2Cr(at.%)合金的超塑性。发现齐纳-霍洛蒙相对公式存在严重的偏转。根据真超塑应力和真应变曲线,得到挠度值n=-7.46和B=1439MPa,说明已经超过了n>0的极限,需要用负号表示。这说明它符合n越小超塑性越好的原理,但它变成负数的问题需要引起同行的注意,同时B是一个更好的匹配。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信