Analysis of unidirectional aligned Banana and Glass fiber reinforced polyester composite for tensile and flexural strength

IF 0.1 Q4 POLYMER SCIENCE
Vatsal Maisuriya, P. Jain, H. Jariwala, Damyanti G. Badagha
{"title":"Analysis of unidirectional aligned Banana and Glass fiber reinforced polyester composite for tensile and flexural strength","authors":"Vatsal Maisuriya, P. Jain, H. Jariwala, Damyanti G. Badagha","doi":"10.37591/jopc.v8i2.3936","DOIUrl":null,"url":null,"abstract":"The hybrid composite can be set up by utilizing at least two fiber fortifications in the composite. Here the hybrid composite was set up by utilizing banana/glass fiber. In addition, fiber volume loading was 40%. The tensile test and flexural test were preceded according to ASTM D3039 and ASTM D790 separately. The results show that 5% treated fiber shows higher properties than non-treated fiber composite. NaOH treated banana fiber with glass fiber composite shows higher quality as compared with non-treated in unidirectional continuous fiber reinforced composite.","PeriodicalId":41357,"journal":{"name":"Journal of Polymer & Composites","volume":null,"pages":null},"PeriodicalIF":0.1000,"publicationDate":"2020-08-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Polymer & Composites","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.37591/jopc.v8i2.3936","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"POLYMER SCIENCE","Score":null,"Total":0}
引用次数: 5

Abstract

The hybrid composite can be set up by utilizing at least two fiber fortifications in the composite. Here the hybrid composite was set up by utilizing banana/glass fiber. In addition, fiber volume loading was 40%. The tensile test and flexural test were preceded according to ASTM D3039 and ASTM D790 separately. The results show that 5% treated fiber shows higher properties than non-treated fiber composite. NaOH treated banana fiber with glass fiber composite shows higher quality as compared with non-treated in unidirectional continuous fiber reinforced composite.
单向排列香蕉和玻璃纤维增强聚酯复合材料的拉伸和弯曲强度分析
混合复合材料可以通过在复合材料中利用至少两种纤维强化物来建立。本文以香蕉/玻璃纤维为原料,建立了一种复合材料。此外,纤维体积负荷为40%。拉伸试验和弯曲试验分别按照ASTM D3039和ASTM D790进行。结果表明,经5%处理的纤维复合材料性能优于未处理的纤维复合材料。NaOH处理后的香蕉纤维与玻璃纤维复合材料的质量比未经NaOH处理的单向连续纤维增强复合材料高。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
2
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信