{"title":"Corrosion behaviour and heat treatment in low-melting Ni-Cu-Mn alloy.","authors":"K Wakasa, M Yamaki","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>The appropriate procedure to improve corrosive property of B-grain in Ni-Cu-Mn casting alloy was to do the heat treatment at 350 degrees C for 6 hrs, because heavy corrosive behaviour was observed for only B-grain in dendritic A-grain, disk-like B-grain and very large C-grain. Then, new grain with corrosion-resistance appeared at previous location of B-grain.</p>","PeriodicalId":76541,"journal":{"name":"Shika rikogaku zasshi. Journal of the Japan Society for Dental Apparatus and Materials","volume":"22 60","pages":"295-8"},"PeriodicalIF":0.0000,"publicationDate":"1981-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Shika rikogaku zasshi. Journal of the Japan Society for Dental Apparatus and Materials","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The appropriate procedure to improve corrosive property of B-grain in Ni-Cu-Mn casting alloy was to do the heat treatment at 350 degrees C for 6 hrs, because heavy corrosive behaviour was observed for only B-grain in dendritic A-grain, disk-like B-grain and very large C-grain. Then, new grain with corrosion-resistance appeared at previous location of B-grain.