{"title":"Bond strength of self-adhesive resin cement to definitive resin crown materials manufactured by additive and subtractive methods.","authors":"Elifnaz Ozen Sutuven, Nuray Capa Yildirim","doi":"10.4012/dmj.2024-111","DOIUrl":null,"url":null,"abstract":"<p><p>The aim was to compare different surface pretreatments on definitive resin crown materials manufactured additively or subtractively in terms of shear bond strength (SBS) values. Seven subgroups (n=10) were formed from additively manufactured VarseoSmile Crown Plus (VS) and subtractively manufactured Cerasmart270 blocks (CS) according to different surface pretreatments applied; sandblasting (subgroup SB), hydrofluoric acid (subgroup HF), Multi Primer (subgroup MP), subgroup SB-HF, subgroup SB-MP, subgroup SB-HF-MP, and control subgroup. A 3-mm-diameter composite was cemented onto each sample by self-adhesive resin cement. SBS values were measured and failure modes were analyzed after thermocycling. Data were analyzed with two-way ANOVA and Tukey HSD tests. The mean SBS value of VS was found significantly higher than CS (p<0.001). Subgroups SB-HF-MP, HF, SB-MP, and MP of VS exhibited the highest SBS values (p<0.001). The VS exhibited mostly cohesive failure, while CS exhibited mostly adhesive failure.</p>","PeriodicalId":11065,"journal":{"name":"Dental materials journal","volume":" ","pages":"41-51"},"PeriodicalIF":1.9000,"publicationDate":"2025-01-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Dental materials journal","FirstCategoryId":"5","ListUrlMain":"https://doi.org/10.4012/dmj.2024-111","RegionNum":4,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2024/12/7 0:00:00","PubModel":"Epub","JCR":"Q2","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0
Abstract
The aim was to compare different surface pretreatments on definitive resin crown materials manufactured additively or subtractively in terms of shear bond strength (SBS) values. Seven subgroups (n=10) were formed from additively manufactured VarseoSmile Crown Plus (VS) and subtractively manufactured Cerasmart270 blocks (CS) according to different surface pretreatments applied; sandblasting (subgroup SB), hydrofluoric acid (subgroup HF), Multi Primer (subgroup MP), subgroup SB-HF, subgroup SB-MP, subgroup SB-HF-MP, and control subgroup. A 3-mm-diameter composite was cemented onto each sample by self-adhesive resin cement. SBS values were measured and failure modes were analyzed after thermocycling. Data were analyzed with two-way ANOVA and Tukey HSD tests. The mean SBS value of VS was found significantly higher than CS (p<0.001). Subgroups SB-HF-MP, HF, SB-MP, and MP of VS exhibited the highest SBS values (p<0.001). The VS exhibited mostly cohesive failure, while CS exhibited mostly adhesive failure.
期刊介绍:
Dental Materials Journal is a peer review journal published by the Japanese Society for Dental Materials and Devises aiming to introduce the progress of the basic and applied sciences in dental materials and biomaterials. The dental materials-related clinical science and instrumental technologies are also within the scope of this journal. The materials dealt include synthetic polymers, ceramics, metals and tissue-derived biomaterials. Forefront dental materials and biomaterials used in developing filed, such as tissue engineering, bioengineering and artificial intelligence, are positively considered for the review as well. Recent acceptance rate of the submitted manuscript in the journal is around 30%.