Effect of Different Liquids and Thermal Aging Procedures on the Shear Bond Strength of APC II, APC Flash-Free, and Conventional Ceramic Brackets: An In Vitro Study.

IF 0.8 Q4 DENTISTRY, ORAL SURGERY & MEDICINE
Hasan Camcı, Şeyda Canbaz Çevik
{"title":"Effect of Different Liquids and Thermal Aging Procedures on the Shear Bond Strength of APC II, APC Flash-Free, and Conventional Ceramic Brackets: An <i>In Vitro</i> Study.","authors":"Hasan Camcı, Şeyda Canbaz Çevik","doi":"10.4274/TurkJOrthod.2023.2023.5","DOIUrl":null,"url":null,"abstract":"<p><strong>Objective: </strong>The purpose of this study was to compare the effects of cherry juice, coffee, coke, gastric acid, and the thermo-aging procedure (TAP) on the shear bond strength (SBS) of APC II, APC flash-free, and conventional ceramic brackets.</p><p><strong>Methods: </strong>A total of 180 human premolar teeth were randomly divided into three major groups according to the type of ceramic bracket. Then, six subgroups (n=10) were established from each major group: Group 1: control; Group 2: only TAP; Group 3: 72 hours of cherry juice exposure + TAP; Group 4: 72 hours of coffee exposure + TAP; Group 5: 72 hours of coke exposure + TAP; and Group 6: 24 hours gastric acid exposure + TAP. SBS was assessed for each specimen using a universal test device, and the adhesive remnant index (ARI) was scored under a light microscope. Kruskal-Wallis and post-hoc Tamhane tests were used to analyze the data.</p><p><strong>Results: </strong>Among the control groups, the highest SBS value belonged to conventional ceramic brackets (p<0.01). SBS values for all groups decreased as a result of each liquid and TAP. Gastric acid and coke had the greatest detrimental effects on SBS, while TAP had the least negative effects. The SBS values of APC II, APC flash-free, and conventional brackets were found to be statistically insignificant after different liquid exposures and TAP.</p><p><strong>Conclusion: </strong>TAP and various fluids had a negative impact on the SBS value of ceramic brackets. SBS values, however, were still higher than clinically acceptable (8-9 MPa) values, even after exposure to gastric acid and coke.</p>","PeriodicalId":37013,"journal":{"name":"Turkish Journal of Orthodontics","volume":"37 3","pages":"140-145"},"PeriodicalIF":0.8000,"publicationDate":"2024-09-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC11589170/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Turkish Journal of Orthodontics","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4274/TurkJOrthod.2023.2023.5","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0

Abstract

Objective: The purpose of this study was to compare the effects of cherry juice, coffee, coke, gastric acid, and the thermo-aging procedure (TAP) on the shear bond strength (SBS) of APC II, APC flash-free, and conventional ceramic brackets.

Methods: A total of 180 human premolar teeth were randomly divided into three major groups according to the type of ceramic bracket. Then, six subgroups (n=10) were established from each major group: Group 1: control; Group 2: only TAP; Group 3: 72 hours of cherry juice exposure + TAP; Group 4: 72 hours of coffee exposure + TAP; Group 5: 72 hours of coke exposure + TAP; and Group 6: 24 hours gastric acid exposure + TAP. SBS was assessed for each specimen using a universal test device, and the adhesive remnant index (ARI) was scored under a light microscope. Kruskal-Wallis and post-hoc Tamhane tests were used to analyze the data.

Results: Among the control groups, the highest SBS value belonged to conventional ceramic brackets (p<0.01). SBS values for all groups decreased as a result of each liquid and TAP. Gastric acid and coke had the greatest detrimental effects on SBS, while TAP had the least negative effects. The SBS values of APC II, APC flash-free, and conventional brackets were found to be statistically insignificant after different liquid exposures and TAP.

Conclusion: TAP and various fluids had a negative impact on the SBS value of ceramic brackets. SBS values, however, were still higher than clinically acceptable (8-9 MPa) values, even after exposure to gastric acid and coke.

不同液体和热老化程序对 APC II、APC Flash-Free 和传统陶瓷牙托剪切结合强度的影响:体外研究。
研究目的本研究旨在比较樱桃汁、咖啡、可乐、胃酸和热老化程序(TAP)对APC II、APC flash-free和传统陶瓷托槽剪切粘结强度(SBS)的影响:根据陶瓷托槽的类型,将 180 颗人类前磨牙随机分为三大组。然后,从每个大组中设立六个小组(n=10):第 1 组:对照组;第 2 组:仅使用 TAP;第 3 组:接触樱桃汁 72 小时 + TAP;第 4 组:接触咖啡 72 小时 + TAP;第 5 组:接触可乐 72 小时 + TAP;第 6 组:接触胃酸 24 小时 + TAP。使用通用测试装置对每个样本的 SBS 进行评估,并在光学显微镜下对粘附残留指数(ARI)进行评分。数据分析采用 Kruskal-Wallis 检验和 Tamhane 后检验:结果:在对照组中,传统陶瓷托槽的 SBS 值最高(p):TAP和各种液体对陶瓷托槽的SBS值有负面影响。不过,即使暴露于胃酸和焦炭中,SBS 值仍高于临床可接受值(8-9 兆帕)。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Turkish Journal of Orthodontics
Turkish Journal of Orthodontics Dentistry-Orthodontics
CiteScore
2.10
自引率
9.10%
发文量
34
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信