{"title":"EPDM Elastomers as Impact Modifiers for Contaminated, Recycled HDPE","authors":"Stefan Tall, Sigbritt Karlsson, Ann-Christine Albertsson","doi":"10.1177/096739119700500602","DOIUrl":null,"url":null,"abstract":"The value of recycled high-density polyethylene (HDPE) is lowered if it contains impurities of PP, PS or PET, hut the embrittlement (partial loss of ductility and toughness) that arises when HDPE i...","PeriodicalId":20417,"journal":{"name":"Polymers and Polymer Composites","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-05-04","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Polymers and Polymer Composites","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1177/096739119700500602","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The value of recycled high-density polyethylene (HDPE) is lowered if it contains impurities of PP, PS or PET, hut the embrittlement (partial loss of ductility and toughness) that arises when HDPE i...