{"title":"ANALYSIS OF WATER PERFORMANCE OF COATING MORTARS INCORPORATED WITH TIRE RUBBER","authors":"L. Pagoto, J. Akasaki, J. L. Pinheiro Melges, C. Fioriti","doi":"10.7764/ric.00018.21","DOIUrl":null,"url":null,"abstract":"This paper analyzed the behavior of mixed mortars incorporated with rubber from the tire retreading process, based on partial sand substitution. The content of rubber incorporation in the mortars was 5%, 10%, 15%, and 20% by volume. The different granulometries of rubber were denominated as thick (passed through a sieve # 1.19 mm) and fine (passed through a sieve # 0.60 mm). Tests were performed to evaluate water retention, capillary absorption, drying, immersion absorption, water vapor permeability, and permeability to water under pressure. The results showed that the fine rubber was distinguished by its higher retention of water at the contents of 15% and 20%, lower absorption via both capillary and immersion, higher drying capacity, higher permeability to water vapor, and lower permeability to water under pressure.","PeriodicalId":369360,"journal":{"name":"Revista Ingeniería de Construcción","volume":"39 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Revista Ingeniería de Construcción","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.7764/ric.00018.21","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

This paper analyzed the behavior of mixed mortars incorporated with rubber from the tire retreading process, based on partial sand substitution. The content of rubber incorporation in the mortars was 5%, 10%, 15%, and 20% by volume. The different granulometries of rubber were denominated as thick (passed through a sieve # 1.19 mm) and fine (passed through a sieve # 0.60 mm). Tests were performed to evaluate water retention, capillary absorption, drying, immersion absorption, water vapor permeability, and permeability to water under pressure. The results showed that the fine rubber was distinguished by its higher retention of water at the contents of 15% and 20%, lower absorption via both capillary and immersion, higher drying capacity, higher permeability to water vapor, and lower permeability to water under pressure.
掺轮胎橡胶涂层砂浆的水性能分析
本文在部分砂替代的基础上,分析了轮胎翻新过程中掺加橡胶的混合砂浆的性能。砂浆中橡胶掺入量按体积计分别为5%、10%、15%和20%。橡胶的不同粒度被命名为厚(通过1.19 mm的筛子)和细(通过0.60 mm的筛子)。进行了保水性、毛细吸水性、干燥性、浸没吸水性、水蒸气渗透性和压力下的透水性试验。结果表明:细胶在含量为15%和20%时具有较高的保水率、较低的毛管吸收率和浸渍吸收率、较高的干燥能力、较高的水蒸气渗透性和较低的压水渗透性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信