{"title":"ABOUT REQUIREMENTS TO PLUGGING MATERIALS AND TO TUBING TECHNOLOGY FOR THE CASING COLUMNS WORKING IN EXTREME CONDITIONS","authors":"A. Kabdushev, F. Agzamov","doi":"10.37878/2708-0080/2022-3.04","DOIUrl":null,"url":null,"abstract":"The most vulnerable elements of the well lining is cement paste in injection wells and the lower parts of the intermediate and surface casings, which suggests the need for the study of additional requirements to plugging materials and lining technology of the specified lining elements. Analysis shows that the main number of workover happens for the share of injection wells, and the number of detected violations in injection wells which is more than an order of magnitude exceeds the corresponding figures for the production casing. Samples of cement stone, selected from the injection and production wells showed that in injection wells, the cement stone collapses in 4-5 years.The mechanism and kinetic process of destruction of cement stone under the influence of leaching was considered and the ways of increasing the durability of linings in injection wells were shown. Leaching corrosion processes in injection wells strengthens during the formation of cracks in the cement stone as a result of technological operation inside the casing string. The most dangerous technological operations are; perforation and deepening of the well. In order to obtain high-quality well anchoring, it is inevitable to regulate the basic properties of cement mortars with the help of various chemical reagents. At the same time, the filtration characteristics (water output and water separation), setting time, pumpability, rheological parameters, as well as the properties of the resulting stone require correction most often in grouting solutions It is shown that for plugging materials, the most preferred way to increase the resistance of grouting stone to dynamic loads is dispersed reinforcement, which can be effectively regulated by the most important characteristics of cement slurries and cement stone can be obtained from them. Studies have been conducted on the influence of basalt fiber and polyamide fiber on the basic physical and mechanical properties of the resulting stone, such as the strength of cement stone, deformation of cement stone during destruction, the specific impact strength of Portland cement stone, as well as the permeability of cement stone. Studies have shown positive results of the addition of basalt fiber at concentrations up to 2%.","PeriodicalId":272594,"journal":{"name":"Neft i gaz","volume":"45 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-06-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Neft i gaz","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.37878/2708-0080/2022-3.04","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

The most vulnerable elements of the well lining is cement paste in injection wells and the lower parts of the intermediate and surface casings, which suggests the need for the study of additional requirements to plugging materials and lining technology of the specified lining elements. Analysis shows that the main number of workover happens for the share of injection wells, and the number of detected violations in injection wells which is more than an order of magnitude exceeds the corresponding figures for the production casing. Samples of cement stone, selected from the injection and production wells showed that in injection wells, the cement stone collapses in 4-5 years.The mechanism and kinetic process of destruction of cement stone under the influence of leaching was considered and the ways of increasing the durability of linings in injection wells were shown. Leaching corrosion processes in injection wells strengthens during the formation of cracks in the cement stone as a result of technological operation inside the casing string. The most dangerous technological operations are; perforation and deepening of the well. In order to obtain high-quality well anchoring, it is inevitable to regulate the basic properties of cement mortars with the help of various chemical reagents. At the same time, the filtration characteristics (water output and water separation), setting time, pumpability, rheological parameters, as well as the properties of the resulting stone require correction most often in grouting solutions It is shown that for plugging materials, the most preferred way to increase the resistance of grouting stone to dynamic loads is dispersed reinforcement, which can be effectively regulated by the most important characteristics of cement slurries and cement stone can be obtained from them. Studies have been conducted on the influence of basalt fiber and polyamide fiber on the basic physical and mechanical properties of the resulting stone, such as the strength of cement stone, deformation of cement stone during destruction, the specific impact strength of Portland cement stone, as well as the permeability of cement stone. Studies have shown positive results of the addition of basalt fiber at concentrations up to 2%.
介绍了在极端条件下工作的套管柱对封堵材料和油管工艺的要求
井衬最脆弱的部位是注水井内的水泥浆以及中间和地面套管的下部,因此有必要研究对特定衬套的封堵材料和衬管工艺的附加要求。分析表明,修井数量主要发生在注水井中,注水井中检测到的违规数量超过生产套管的相应数量一个数量级以上。从注采井和生产井中选取的水泥石样品表明,在注采井中,水泥石在4-5年内坍塌。分析了浸出作用下水泥石破坏的机理和动力学过程,提出了提高注水井衬砌耐久性的途径。在注水井中,由于套管柱内部的工艺操作,在水泥石裂缝形成过程中,浸出腐蚀过程会加剧。最危险的技术操作是;射孔和井深。为了获得高质量的井锚,必须借助各种化学试剂调节水泥砂浆的基本性能。同时,过滤特性(出水量和分离水量)、凝结时间、可泵性、流变参数以及所得石材的性能在注浆溶液中最需要修正。由此可见,对于堵漏材料而言,增加注浆石材抗动荷载的最优选方法是分散加固;这可以通过水泥浆和水泥石最重要的特性得到有效的调节。研究了玄武岩纤维和聚酰胺纤维对水泥石的基本物理力学性能的影响,如水泥石的强度、水泥石破坏时的变形、波特兰水泥石的比冲击强度、水泥石的渗透性等。研究表明,添加浓度高达2%的玄武岩纤维具有积极的效果。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信