Fabrication of Gd2O3/PSF Membranes via Aqueous Phase Inversion Method

Ayşe Gul, Dilek Şenol Arslan, N. Uzal
{"title":"Fabrication of Gd2O3/PSF Membranes via Aqueous Phase Inversion Method","authors":"Ayşe Gul, Dilek Şenol Arslan, N. Uzal","doi":"10.17350/hjse19030000269","DOIUrl":null,"url":null,"abstract":"This study aimed to investigate the effect of Gadolinium oxide (Gd2O3) concentration (0.5%, 1%, and 2%) on the performance of polysulfone (PSF) membrane. The membranes were fabricated by a common phase inversion method. The performance of membranes was determined based on pure water flux, bovine serum albumin (BSA) permeation test. These fabricated membranes were characterized by FTIR and contact angle measurements. The highest BSA rejection was 53%. The optimum membrane (2 % wt Gd2O3 /17 % wt PSF) in this study was determined by PSF 17% which successfully exhibited 53% rejection with filtrate flux for about 8.7 L/m2.h at a pressure of 10 bar.","PeriodicalId":285705,"journal":{"name":"Hittite Journal of Science and Engineering","volume":"11 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-09-28","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Hittite Journal of Science and Engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17350/hjse19030000269","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

This study aimed to investigate the effect of Gadolinium oxide (Gd2O3) concentration (0.5%, 1%, and 2%) on the performance of polysulfone (PSF) membrane. The membranes were fabricated by a common phase inversion method. The performance of membranes was determined based on pure water flux, bovine serum albumin (BSA) permeation test. These fabricated membranes were characterized by FTIR and contact angle measurements. The highest BSA rejection was 53%. The optimum membrane (2 % wt Gd2O3 /17 % wt PSF) in this study was determined by PSF 17% which successfully exhibited 53% rejection with filtrate flux for about 8.7 L/m2.h at a pressure of 10 bar.
水相转化法制备Gd2O3/PSF膜
本研究旨在探讨氧化钆(Gd2O3)浓度(0.5%,1%和2%)对聚砜(PSF)膜性能的影响。膜是用普通的相转化法制备的。通过纯水通量、牛血清白蛋白(BSA)渗透试验测定膜的性能。用FTIR和接触角测量对制备的膜进行了表征。BSA排斥反应最高为53%。本研究的最佳膜(2% wt Gd2O3 / 17% wt PSF)由PSF 17%确定,在10 bar的压力下,滤液通量约为8.7 L/m2.h,成功地达到53%的截留率。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信