DEVELOPMENT OF A PREMIUM COLD MIX ASPHALT

M. Herez, Hassan Al Nageim, J. Richardson, Sommerville Wright
{"title":"DEVELOPMENT OF A PREMIUM COLD MIX ASPHALT","authors":"M. Herez, Hassan Al Nageim, J. Richardson, Sommerville Wright","doi":"10.30572/2018/kje/140303","DOIUrl":null,"url":null,"abstract":"Cold mix asphalt produced using conventional emulsion and limestone filler has three main disadvantages, namely low early strength due to high amount of water within the mix, long curing time ranging from 2-24 months and high air voids content. In this study, the effect of a novel technology for producing high-quality cold mix asphalt using modified bitumen emulsion has been investigated in terms of indirect tensile stiffness modulus. the effect of a novel technology for homogenizing a bitumen emulsion on its viscosity, particle size and particle size distribution has been investigated. Ultrasound technology has been used to reduce the viscosity and the size of the bitumen droplets. Different samples of cationic bitumen emulsion (C50B4) have been prepared with different treatment durations (0, 5, 7, 10, 12.5, 15, 30, 45 and 60) min. The results have shown a reduction in the viscosity of the bitumen emulsion at treatment times from 5-15 min. The viscosity has been decreased by 28% after 10 min treatment for the emulsion compared to the untreated sample. This reduction indicated a uniform droplet size distribution. In addition, the particle size measurements revealed that the 7 min treatment showed a significant reduction in the D 50 , which was 84.5%, D 10 , was 85.89%, and D 90 was 90.28% compared to the untreated bitumen emulsion. The results reported contains a comparison between the viscosity of the emulsions, and the indirect tensile stiffness modulus of a control conventional cold mix asphalt and the new high quality cold mix asphalt with low viscosity. Interestingly, the reduction of the 28% in the viscosity of the new emulsion causes an improvement of the indirect tensile stiffness modulus to 216%, which indicates an outstanding achievement.","PeriodicalId":123515,"journal":{"name":"Kufa Journal of Engineering","volume":"69 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-07-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Kufa Journal of Engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30572/2018/kje/140303","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Cold mix asphalt produced using conventional emulsion and limestone filler has three main disadvantages, namely low early strength due to high amount of water within the mix, long curing time ranging from 2-24 months and high air voids content. In this study, the effect of a novel technology for producing high-quality cold mix asphalt using modified bitumen emulsion has been investigated in terms of indirect tensile stiffness modulus. the effect of a novel technology for homogenizing a bitumen emulsion on its viscosity, particle size and particle size distribution has been investigated. Ultrasound technology has been used to reduce the viscosity and the size of the bitumen droplets. Different samples of cationic bitumen emulsion (C50B4) have been prepared with different treatment durations (0, 5, 7, 10, 12.5, 15, 30, 45 and 60) min. The results have shown a reduction in the viscosity of the bitumen emulsion at treatment times from 5-15 min. The viscosity has been decreased by 28% after 10 min treatment for the emulsion compared to the untreated sample. This reduction indicated a uniform droplet size distribution. In addition, the particle size measurements revealed that the 7 min treatment showed a significant reduction in the D 50 , which was 84.5%, D 10 , was 85.89%, and D 90 was 90.28% compared to the untreated bitumen emulsion. The results reported contains a comparison between the viscosity of the emulsions, and the indirect tensile stiffness modulus of a control conventional cold mix asphalt and the new high quality cold mix asphalt with low viscosity. Interestingly, the reduction of the 28% in the viscosity of the new emulsion causes an improvement of the indirect tensile stiffness modulus to 216%, which indicates an outstanding achievement.
优质冷拌沥青的研制
使用常规乳化液和石灰石填料生产的冷拌沥青有三个主要缺点,即由于混合料中含水量高,早期强度低,养护时间长(2-24个月),空隙率高。在本研究中,从间接拉伸刚度模量的角度研究了用改性沥青乳液生产高质量冷拌沥青的新技术的效果。研究了一种均匀化沥青乳液的新工艺对沥青乳液粘度、粒径和粒径分布的影响。超声技术已被用于降低沥青滴的粘度和尺寸。用不同的处理时间(0、5、7、10、12.5、15、30、45和60)min制备了不同的阳离子沥青乳液(C50B4)样品。结果表明,处理时间为5-15 min时,沥青乳液的粘度有所降低。与未处理样品相比,处理10 min后,乳液的粘度降低了28%。这种减小表明液滴尺寸分布均匀。此外,粒径测量结果表明,与未经处理的沥青乳液相比,处理7 min后的d50、d10和d90分别降低了84.5%、85.89%和90.28%。结果包括乳剂粘度、常规冷拌沥青与新型低粘度优质冷拌沥青的间接拉伸刚度模量的比较。有趣的是,新乳液的黏度降低28%,导致间接拉伸刚度模量提高到216%,这是一个突出的成就。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信