M. Ramírez-Como, E. Moustafa, A. A. A. Torimtubun, José G. Sánchez, J. Pallarès, L. Marsal
{"title":"Preliminary Study of the Degradation of PM6:Y7-based Solar Cells","authors":"M. Ramírez-Como, E. Moustafa, A. A. A. Torimtubun, José G. Sánchez, J. Pallarès, L. Marsal","doi":"10.1109/LAEDC54796.2022.9908202","DOIUrl":null,"url":null,"abstract":"In this work, we report a degradation study of high-efficiency organic solar cells (OSCs). The active layer uses PM6 as a donor and Y7 as an acceptor material, respectively. High performance of the PM6:Y7-based device is achieved with the power conversion efficiency (PCE) of up to 17.3% under 1 sun illumination for the fresh device. To gain a better understanding of PM6:Y7 stability, we developed the analysis of the degradation process over the storage time. The PCE of the device decreased to 82% of the initial PCE after 888 h. The electrical parameters during the degradation process were extracted from the current density – voltage characteristics (J–V) under light and dark conditions.","PeriodicalId":276855,"journal":{"name":"2022 IEEE Latin American Electron Devices Conference (LAEDC)","volume":"6 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-07-04","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2022 IEEE Latin American Electron Devices Conference (LAEDC)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/LAEDC54796.2022.9908202","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
In this work, we report a degradation study of high-efficiency organic solar cells (OSCs). The active layer uses PM6 as a donor and Y7 as an acceptor material, respectively. High performance of the PM6:Y7-based device is achieved with the power conversion efficiency (PCE) of up to 17.3% under 1 sun illumination for the fresh device. To gain a better understanding of PM6:Y7 stability, we developed the analysis of the degradation process over the storage time. The PCE of the device decreased to 82% of the initial PCE after 888 h. The electrical parameters during the degradation process were extracted from the current density – voltage characteristics (J–V) under light and dark conditions.