{"title":"Polymer Modification Exploiting Stable Nitrile N-Oxide","authors":"Y. Koyama, Akishige Seo, T. Takata","doi":"10.2324/GOMU.84.111","DOIUrl":null,"url":null,"abstract":"This paper describes the powerful practical modification method of elastomers with unsaturated bonds exploiting kinetically stabilized nitrile N-oxides. The stable nitrile N-oxides enable the efficient 1,3-dipolar cycloaddition to both internal olefin and nitrile groups incorporating into versatile elastomers such as acrylonitrile butadiene rubber (NBR), natural rubber (NR), and ethylene-propylene-diene terpolymer (EPDM) to give the corresponding hetero aromatics-containing polymers. The reaction features i) catalyst-free procedure, ii) versatile applicability to various elastomers, iii) high yield, iv) high regio-selectivity, v) no by-product, and vi) remarkable acceleration of reaction rate under solvent-free condition. The scope and limitation of the modification reaction are discussed in detail.","PeriodicalId":405949,"journal":{"name":"Journal of the Society of Rubber Industry,Japan","volume":"42 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2011-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"13","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of the Society of Rubber Industry,Japan","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2324/GOMU.84.111","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 13
Abstract
This paper describes the powerful practical modification method of elastomers with unsaturated bonds exploiting kinetically stabilized nitrile N-oxides. The stable nitrile N-oxides enable the efficient 1,3-dipolar cycloaddition to both internal olefin and nitrile groups incorporating into versatile elastomers such as acrylonitrile butadiene rubber (NBR), natural rubber (NR), and ethylene-propylene-diene terpolymer (EPDM) to give the corresponding hetero aromatics-containing polymers. The reaction features i) catalyst-free procedure, ii) versatile applicability to various elastomers, iii) high yield, iv) high regio-selectivity, v) no by-product, and vi) remarkable acceleration of reaction rate under solvent-free condition. The scope and limitation of the modification reaction are discussed in detail.
本文介绍了利用动力学稳定的腈- n -氧化物对不饱和键弹性体进行改性的实用方法。稳定的腈- n -氧化物使得高效的1,3-偶极环加成到内部烯烃和腈基上,形成通用弹性体,如丙烯腈-丁二烯橡胶(NBR)、天然橡胶(NR)和乙烯-丙烯-二烯三元聚合物(EPDM),从而得到相应的含杂芳烃聚合物。该反应具有以下特点:1)无催化剂;2)适用于多种弹性体;3)产率高;4)区域选择性高;5)无副产物;6)无溶剂条件下反应速度明显加快。详细讨论了改性反应的范围和局限性。