{"title":"PENGARUH PENAMBAHAN MATERIAL LIMBAH PECAHAN BATU BATA DAN PECAHAN GENTENG SEBAGAI SUBTITUSI AGREGAT KASAR TERHADAP KUAT TEKAN BETON","authors":"Thasya Amelia, Henggar Risa Destania, Febryandi Febryandi","doi":"10.35194/momen.v5i2.2563","DOIUrl":null,"url":null,"abstract":"Abstract: the waste of fraction bricks and tile fragments for mixing in concrete in Indonesia is stil not widely used in heavy-duty construction buildings. For this reason, this study aims to determine the compressive strenght of concrete by utilizing waste brick and tile fragments as a substitute for coarse aggregate. This test has several stages, namelu material testing, making test objects, testing concrete compressive strength, and analyzing test results. In this test, the specimens were molded using a cylinder with a mixture of substituting brick fragments and tile framents against coarse aggregate with variasions of 5%, 10% and 15%. The results of the compressive strenght test on norma unmixed concrete with a 5% age of 28 days obtained a value of 16,6 MPa, on concrete with a 5% variation of brick and tile with an age of 28 days a value of 12,41 MPa was obtained, on a concrete variatio of 10% brick an tile. The obtained value is 11,98 MPa, and in the 15% variation concrete mixture of brick and tile, the value is 11,54MPa. Keywords: Compressive Strength of Concrete, Coarse Aggregate, Waste fractions Brick and Tile. Abstrak: Limbah pecahan batu bata dan pecahan genteng untuk campuran dalam beton di Indonesia memang masih belum banyak untuk digunakan dalam bangunan kontruksi yang terbeban. Untuk itu penelitian ini bertujuan untuk mengetahui kuat tekan beton dengan memanfaatkan limbah pecahan batu bata dan pecahan genteng sebagai subtitusi agregat kasar. Pengujian ini ada beberapa tahapan, yaitu pengujian material, pembuatan benda uji, pengujian kuat tekan beton, dan analisa hasil pengujian. Pada pengujian ini benda uji dicetak menggunakan silinder dengan campuran subtitusi pecahan batu bata dan pecahan genteng terhadap agregat kasar dengan variasi 5%,10%dan 15%. Hasil uji kuat tekan pada beton normal tanpa campuran dengan umur 28 hari didapat nilai sebesar 16,6 MPa, pada beton dengan variasi 5% bata dan genteng dengan umur 28 hari didapat nilai sebesar 12,41 MPa, pada beton variasi bata dan genteng 10% didapat sebesar 11,98 MPa, dan pada beton variasi 15% campuran bata dan genteng didapat nilai sebesar 11,54 MPa. Kata kunci: : Kuat Tekan Beton, Agregat kasar, Limbah Pecahan bata dan pecahan genteng. ","PeriodicalId":246778,"journal":{"name":"JURNAL MOMEN TEKNIK SIPIL","volume":"25 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-12-06","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"JURNAL MOMEN TEKNIK SIPIL","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.35194/momen.v5i2.2563","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
Abstract: the waste of fraction bricks and tile fragments for mixing in concrete in Indonesia is stil not widely used in heavy-duty construction buildings. For this reason, this study aims to determine the compressive strenght of concrete by utilizing waste brick and tile fragments as a substitute for coarse aggregate. This test has several stages, namelu material testing, making test objects, testing concrete compressive strength, and analyzing test results. In this test, the specimens were molded using a cylinder with a mixture of substituting brick fragments and tile framents against coarse aggregate with variasions of 5%, 10% and 15%. The results of the compressive strenght test on norma unmixed concrete with a 5% age of 28 days obtained a value of 16,6 MPa, on concrete with a 5% variation of brick and tile with an age of 28 days a value of 12,41 MPa was obtained, on a concrete variatio of 10% brick an tile. The obtained value is 11,98 MPa, and in the 15% variation concrete mixture of brick and tile, the value is 11,54MPa. Keywords: Compressive Strength of Concrete, Coarse Aggregate, Waste fractions Brick and Tile. Abstrak: Limbah pecahan batu bata dan pecahan genteng untuk campuran dalam beton di Indonesia memang masih belum banyak untuk digunakan dalam bangunan kontruksi yang terbeban. Untuk itu penelitian ini bertujuan untuk mengetahui kuat tekan beton dengan memanfaatkan limbah pecahan batu bata dan pecahan genteng sebagai subtitusi agregat kasar. Pengujian ini ada beberapa tahapan, yaitu pengujian material, pembuatan benda uji, pengujian kuat tekan beton, dan analisa hasil pengujian. Pada pengujian ini benda uji dicetak menggunakan silinder dengan campuran subtitusi pecahan batu bata dan pecahan genteng terhadap agregat kasar dengan variasi 5%,10%dan 15%. Hasil uji kuat tekan pada beton normal tanpa campuran dengan umur 28 hari didapat nilai sebesar 16,6 MPa, pada beton dengan variasi 5% bata dan genteng dengan umur 28 hari didapat nilai sebesar 12,41 MPa, pada beton variasi bata dan genteng 10% didapat sebesar 11,98 MPa, dan pada beton variasi 15% campuran bata dan genteng didapat nilai sebesar 11,54 MPa. Kata kunci: : Kuat Tekan Beton, Agregat kasar, Limbah Pecahan bata dan pecahan genteng.
文摘:印尼用于混凝土搅拌的分块砖和瓦片废料在重型建筑中应用还不广泛。因此,本研究旨在利用废砖瓦碎片代替粗骨料确定混凝土的抗压强度。该试验分为几个阶段,即材料试验、制作试验对象、测试混凝土抗压强度和分析试验结果。在本试验中,使用圆柱体将砖碎片和瓦碎片的混合物与变化为5%,10%和15%的粗骨料混合成型。在5%龄期为28天的普通未拌混凝土上进行抗压强度试验,其抗压强度值为16.6 MPa,在5%龄期为28天的砖瓦混凝土上进行抗压强度试验,其抗压强度值为12.41 MPa,在10%龄期为砖瓦的混凝土上进行抗压强度试验。得到的值为11,98 MPa,在15%变化的砖瓦混凝土混合料中,该值为11,54MPa。关键词:混凝土抗压强度,粗骨料,废渣砖瓦摘要:lingbah pecahan batu bata dan pecahan genteng untuk campuran dalam beton di Indonesia mamang masih belum banyak untuk digunakan dalam bangunan kontruksi yang terbeban。Untuk i penelitian ini bertujuan Untuk mengetahui kutekan betdenan menmenfaatkan limbah pecahan batu bata danpecahan genteneng sebagai subtitiusi agregat kasar。penguin ini ada beberapa tahapan, yitu penguin material, penbuatan benda uji, Pengujian kuat tekan beton, dan analisa hasil Pengujian。巴布亚企鹅ini benda uji dicetak menggunakan silinder dengan campuran subtitusi pecahan batu bata dpecahan genteng terhadap聚合kasar dengan变化为5%,10%和15%。夸特Hasil里头tekan篇混凝土正常tanpa campuran dengan umur 28哈里didapat汝sebesar 16日6 MPa,篇混凝土dengan variasi 5%巴塔丹genteng dengan umur 28哈里didapat汝sebesar 12日41 MPa,篇混凝土variasi巴塔丹genteng 10% didapat sebesar 11日98 MPa,丹篇混凝土variasi 15% campuran巴塔丹genteng didapat汝sebesar 11日,54 MPa。Kata kunci: Kuat Tekan Beton, Agregat kasar, Limbah Pecahan bata dan Pecahan genteng。