{"title":"Use of Laser Metal Deposition Technology in Additive Manufacturing of Ni Powder Materials","authors":"P. Sejč, Jan Jaroš, B. Vanko","doi":"10.2478/scjme-2022-0026","DOIUrl":null,"url":null,"abstract":"Abstract The process parameters of the Laser Metal Deposition technology in the production of simple components made of NiCuBSi type metal powder were verified in this paper. A laser head with a coaxial powder supply and argon gas was used in the production. The powder was welded to a S235J2G3 steel plate. The used parameters (heat input 0.25 kJ.mm−1) enabled the production of samples with a minimum porosity (1.2 %) and without the defects (cold joints, pores) between the weld layers.","PeriodicalId":445896,"journal":{"name":"Strojnícky časopis - Journal of Mechanical Engineering","volume":"29 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Strojnícky časopis - Journal of Mechanical Engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2478/scjme-2022-0026","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Abstract The process parameters of the Laser Metal Deposition technology in the production of simple components made of NiCuBSi type metal powder were verified in this paper. A laser head with a coaxial powder supply and argon gas was used in the production. The powder was welded to a S235J2G3 steel plate. The used parameters (heat input 0.25 kJ.mm−1) enabled the production of samples with a minimum porosity (1.2 %) and without the defects (cold joints, pores) between the weld layers.
激光金属沉积技术在Ni粉末材料增材制造中的应用
摘要本文对激光金属沉积技术在NiCuBSi型金属粉末简单部件生产中的工艺参数进行了验证。采用同轴供粉和氩气的激光头进行生产。将粉末焊接到S235J2G3钢板上。所使用的参数(热输入0.25 kJ.mm−1)使样品具有最小的孔隙率(1.2%),并且在焊接层之间没有缺陷(冷接头,气孔)。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信